Update to my case refinishing and questions...
I stripped off the old black paint on the case and tail housing, hot tanked them and they immediately formed a surface rust. My objective is to have a "factory like" finish that doesn't immediately rust. Car will be garage kept, driven weekends in fair weather, but I am in a moist climate.
So my thoughts are to do this:
*degrease (maybe not necessary after hot tank but will do anyway)
*POR-15 rust remover
*POR-15 metal prep
I'm not sure what to do to finish the cast components so they don't rust again. Will POR-15 metal prep be enough, or do I need to do something like a thin coat of ceramic like Jeff suggests or?
Am I on the right track?
Thanks, Andy